Trying to locate GE spec A16B99A1 or A16B99C1
Trying to locate GE spec A16B99A1 or A16B99C1
(OP)
I have been trying to locate a GE material spec A16B99A1 or A16B99C1 called out on a 1984 drawing 1333M60. I have tried google, looked in some of our old GE spec books, asked some approved GE manufacturers but cannot seem to locate anyone with the spec or anyone who is able to identify the material. Can anyone help?





RE: Trying to locate GE spec A16B99A1 or A16B99C1
This material is a carbon filled polyimide.
Tom
RE: Trying to locate GE spec A16B99A1 or A16B99C1
Thanks Tom!
RE: Trying to locate GE spec A16B99A1 or A16B99C1
Tom
RE: Trying to locate GE spec A16B99A1 or A16B99C1
By chance, would you be able to send me that spec via attachment?
RE: Trying to locate GE spec A16B99A1 or A16B99C1
Or perhaps you might know who distributes or sells this material?