INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Fundamentals of Concrete Mix Design

Fundamentals of Concrete Mix Design

Fundamentals of Concrete Mix Design

(OP)
I am putting together a training module for my company entitled Fundamentals of Concrete Mix Design.  Am wondering if anyone has any literature on the topic I could reference in my module?  This training topic is for 0-5 year engineers in the company.

RE: Fundamentals of Concrete Mix Design

Perhaps the best reference for such a training course is "Design and Control of Concrete Mixes", a publication of the Portland Cement Association at the noted website.

RE: Fundamentals of Concrete Mix Design

For PCA - just make sure you don't order their DVD on concrete inspection - a primer for new engineers.  I was embarrassed - having paid big $$ and seeing some video.  In my view, a bit amateurish (as in my bad spelling today) - good to see you back Ron!!

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources