Corrosive sulfur
Corrosive sulfur
(OP)
Hi all,
The problem with corrosive sulfur in the oil, especially in Power Transformers and Reactors is known.
Do you have any expierence with it? Maybe problems?
Regards,
Peter
The problem with corrosive sulfur in the oil, especially in Power Transformers and Reactors is known.
Do you have any expierence with it? Maybe problems?
Regards,
Peter






RE: Corrosive sulfur
http://www.doble.com/newsletter/pdf/6_3.pdf
RE: Corrosive sulfur
This is not exactly as you wrote. I agree with specific time period but I've heard about transformer failure because of corrosive sulfur in Norway..
I'm from Poland. We are also trying to do some research in our units. We suppose we have problem with several units.
That's I'm looking for some more information.
Peter
RE: Corrosive sulfur
RE: Corrosive sulfur
I have hands on experience on this problem and studying the reports from all over the world on this issue since it was first reportd. I know about problem in Norway,but not anything fronm Poland.If you say exacly what you want to know,probably, I can throw some light.