pipe weld callout
pipe weld callout
(OP)
What would be the best callout to weld the pipe to the triangular piece?
pipe: 300 series stainless, 1.25 OD, 1.125 ID,
trinagular plate: 300 series stainless, 0.25 thick.
Thanks!
pipe: 300 series stainless, 1.25 OD, 1.125 ID,
trinagular plate: 300 series stainless, 0.25 thick.
Thanks!





RE: pipe weld callout
"What is the proper call-out for the parts shown, with no further joint preparation?"
or
"What would be the best joint for welding these two things together?"
If the former, I think it's a flare-bevel. If the later, much more information is needed.