INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

PMMA Molding

PMMA Molding

PMMA Molding

(OP)
HI experts ,
I have a problem with pmma part , that is about some "Air trap"  , some are inside and some are at surface and I preheat the resin perfectly ,
now how Should I adjust setting such as : Speed , press and time of Injection ,charging ......

Thanks

RE: PMMA Molding

Is the material dry.

Are you sure it is air trap and not contraction void.

Without seeing the part and fault, I will take a SWAG at it just for fun.

Try injecting fairly slow with a fairly warm mould, use as much pressure as you can without causing flash. Make sure the gate and runner are big enough.

Hold up injection pressure until you get no more weight gain from extra time.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.
 

RE: PMMA Molding

Oh

And read the troubleshooting guides that come with the machine and will be provide on request from the raw materials supplier.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.
 

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources