thermal creep data about T91 (9Cr-1Mo-V - Nb)
thermal creep data about T91 (9Cr-1Mo-V - Nb)
(OP)
Hi,
I'm searching data about thermal creep of T91 and/or some correlation describing it.
I'm finding a lot of "stress-time to rupture" and microstuctural evolution data but almost anything about "strain-time" or "strain rate-time" @ a given temperature.
Could someone help me in this data collection?
thank you!!
Alf
I'm searching data about thermal creep of T91 and/or some correlation describing it.
I'm finding a lot of "stress-time to rupture" and microstuctural evolution data but almost anything about "strain-time" or "strain rate-time" @ a given temperature.
Could someone help me in this data collection?
thank you!!
Alf





RE: thermal creep data about T91 (9Cr-1Mo-V - Nb)
If you want strain-time data, one paper that I found on the public domain was authored by Robert W. Swindeman who was with Oak Ridge National Lab (ORNL) before he retired and his son Mike J. Swindeman. The title of this paper - available in powerpoint or word is
"Understanding Damage Mechanisms in Ferritic/Marensitic Steels" presented at the 17th Annual Conference on Fossil Energy Materials, in Baltimore MD, 4/2003.
Grade 91 basically originated from ORNL.
RE: thermal creep data about T91 (9Cr-1Mo-V - Nb)
Ferritic/Martensitic Steels
RE: thermal creep data about T91 (9Cr-1Mo-V - Nb)
http://l
RE: thermal creep data about T91 (9Cr-1Mo-V - Nb)
maybe it will be useful
http://www.metrode.com/docs/news/P92%20Profile.pdf
http://ww
Luis Marques