Do you know of a website where I can find the section properties for SZ sheet piling? In particular I am looking for SZ-22 sheet piling.
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: SZ Sheet Piling
RE: SZ Sheet Piling
Interlock type: H & G
Cold Formed
X-Sect. Area per Foot of Wall: 6.41in^2
Nominal Width per Section: 26.75"
Weight per Lin Ft: 48.6lb
Weight per Sq Ft: 21.8lb
Wall Depth: 9.46"
Web Thickness: 0.375"
Flange Thickness: 0.375"
Moment of Inertia per Foot of Wall: 91.9in^4
Section Modulus per Foot of Wall: 19.3in^3
Surface Area per Lin Ft: 5.75ft^2 (nominal coating area - does not include interlock surfaces)