INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

How to calculate shear and flexural strength of hollow precast beam?

How to calculate shear and flexural strength of hollow precast beam?

How to calculate shear and flexural strength of hollow precast beam?

(OP)
I am involved in a project using hollow precast beam. But I am only familiar with reinforced concrete beam. Can I treat it the same way as concrete beams? How should I deal with those hollow holes which go through all the whole beam length? Can you please also recommend me some good design books on these hollow precast beams?

Thank you very much in advance!

RE: How to calculate shear and flexural strength of hollow precast beam?

It is a more efficient section.  Look at any precast book or even PCI Design Handbook in teh hollow core plank section.  Removing concrete in the middle of the section removes a great deal of dead load and that concrete isn't contributing much to your Igross and overall section properties, that is why it is a more efficient section.

RE: How to calculate shear and flexural strength of hollow precast beam?

It is probably prestressed with 7 or more strands for total section in compression under dead load and a percentage of live load.  Topping ties the adjacent planks together for unit action and more flexural capability.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources