INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

NASGRO 3.0

NASGRO 3.0

NASGRO 3.0

(OP)
I am teaching myself to use NASGRO. I have version 3.0.
I have had success running the program for simple problems ie cracks in skins under pressure loading.
I want to move on to problems with more involved loading but inputing the spectrum is causing problems. I would appreciate it if someone had some input files for problems involving G-A-G cycles that I could get a copy of so that I could see how the data is input into the program.
Your help would be gratefully received.

Thanks
CS

RE: NASGRO 3.0

AFGROW has nothing to do with NASGRO. Many of the crack solutions in NASGRO are in AFGROW; however, almost all of these solutions are in the open literature. So I think it is in error to say that NASGRO is an integral part of AFGROW.

There is something from NASGRO in AFGROW--the material crack growth rate database in NASGRO is one of the options in AFGROW, which has several options for crack growth rates--your own curve, NASGRO's curves, Forman equation, Walker equation, and Harter-T method.

Besides, up until last December (2007), AFGROW was free to users, fully funded by US taxpayers; it will cost something (unknown) in the future.

What's the going rate for entrance into the NASGRO consortium (which gives you access to this formerly free software) now?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources