INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

NACE MR 0175 heat treatment conditions

NACE MR 0175 heat treatment conditions

NACE MR 0175 heat treatment conditions

(OP)
In Par. 3.2 of NACE MR 0175, only a restricted number of heat treatment conditions are allowed: hot rolled, annealed, normalized, normalized and tempered, normalized + austenized + quenched + tempered, austenized + quenched + tempered.
Some heat treatment conditions like thermomechanical rolling or normalizing rolling are not included.
In appendix D, table D1, pipes up to API-5L X65 are considered as acceptable material.  Or practically all X65 material is thermomechanical rolled.
Does someone has more information about the choice of NACE?  

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources