ASTM A182 F22 welding
ASTM A182 F22 welding
(OP)
I am developing a WPS (butt weld) for F22 material. I am looking for the PWHT information for this material, does anyone know where this may be located? (ASME VIII for instance)?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: ASTM A182 F22 welding
I would use the code of construction - piping (B31.x) or ASME Boiler and Pressure Vessel Code (Section I or VIII, Div 1). Section VIII, Div 1 is UCS-56.