INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Virgin PTFE Tubing Pressure-Temperture Derating

Virgin PTFE Tubing Pressure-Temperture Derating

Virgin PTFE Tubing Pressure-Temperture Derating

(OP)
I am looking for a pressure-temperature chart for Virgin PTFE tubing.  Any one know where one is located on the web?  As an alternative does anyone know a published tensile strength for Virgin PTFE at elevated temperatures greater than 73F.  I am looking for tensile strength value for Virgin PTFE per ASTM D1457 at 175F (80C).

RE: Virgin PTFE Tubing Pressure-Temperture Derating

Everything I see suggests around a 30% reduction in pressure rating at 80C, but I do not know of a definitive source for this info.

RE: Virgin PTFE Tubing Pressure-Temperture Derating

(OP)
Thanks GooyatEEE,

Do you have documentation or published data showing the reduction value?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources