PWHT thickness for ASME B31.3
PWHT thickness for ASME B31.3
(OP)
Does any one know if the max. thickness for P-No.1 material not requiring PWHT in Table 331.1.1 in the latest issue of ASME B31.3 is increased from 19 to 20 mm?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
PWHT thickness for ASME B31.3
|
RE: PWHT thickness for ASME B31.3
P1 material
less than or equal to 20 mm = none
greater than 20 mm = 593 - 649 degrees C, 2.4 min / mm