Jigging-Shoveling-Rodding
Jigging-Shoveling-Rodding
(OP)
ASTM C29 has three methods to determine unit weight of aggregate - see thread's title. What experience is in our group to advise which method is most realistic and reasonable for (1) material in stockpile (2) material in tipper (dump truck)? Would like to see what the consensus is.