INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Digital radiography standards and differences in acceptance criteria

Digital radiography standards and differences in acceptance criteria

Digital radiography standards and differences in acceptance criteria

(OP)
We are about to test digital radiography with GE,
so long I have found these standards but I am worried I missing something.
More over I want to know whats the main differences in acceptance criteria

CEN standards
EN 14784-1 : Industrial CR with storage phosphor imaging plates
Part 1 : Classification of systems
EN 14784-2 : Industrial CR with storage phosphor imaging plates
Part 2 : General principles for examination of metals using X-rays and gamma rays

ISO standards
ISO 10042

ASTM standards:
ASTM 2007-00 : Standard Guide for Computed Radiography
ASTM E1936-03(2007): Standard Reference Radiograph for Evaluating the Performance of Radiographic Digitization Systems
ASTM 2033-99 : Standard Practice for Computed Radiography
ASTM 2445-05 : Standard Practice for Qualification and Long-Term Stability of CR systems
ASTM 2446-05 : Standard Practice for Classification of CR systems
ASTM 2339-04 : Digital Imaging and Communication in NDE (DICONDE)
ASTM E 2422: First digital catalogue-light alloy casting

ASME code:
ASME Code Case 2476 : Radiography using phosphor imaging plates

 

RE: Digital radiography standards and differences in acceptance criteria

Ndtmetal,

Not clear what you mean by acceptance criteria.  I think of accetpance criteria was what weld discontinuities are acceptable and which are rejectable.  The acceptance criteria in this sense would not change regardless if you are using film, phosphur plate, or digitizer.

JR97

RE: Digital radiography standards and differences in acceptance criteria

How about the digital equivalents of requirements for film type & radiograph density?

Hg

Eng-Tips policies:  FAQ731-376: Eng-Tips.com Forum Policies

RE: Digital radiography standards and differences in acceptance criteria

(OP)
what about the limit of screen pixel drop off and the optimum screen contras/brightness?

RE: Digital radiography standards and differences in acceptance criteria

(OP)
In film radiography we have classes of films.
What about CR? Is there any standard about the pixel size that should be used in each case?

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources