INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

ASTM A312 with addition of filler metal

ASTM A312 with addition of filler metal

ASTM A312 with addition of filler metal

(OP)
In ASTM A312, welded pipe (for example 304SS) shall be made using an automatic welding process with no addition of filler metal during the welding process.

Can we specify ASTM A312 piping with filler metal? What is the main effect on piping property, using addition of filler metal?

RE: ASTM A312 with addition of filler metal

kissjxp;
No, you cannot indiscriminately add filler metal for this specification. You need to specify another ASTM Specification that is for fusion welded pipe, like ASTM A 358.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources