Stellite 6 to Duplex welds
Stellite 6 to Duplex welds
(OP)
Can Stellite 6 be successfully welded to 2205 Duplex?
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Stellite 6 to Duplex welds
|
RE: Stellite 6 to Duplex welds
RE: Stellite 6 to Duplex welds
Perhaps I should have qualified that you were not talking about a strength weld between duplex and St6. As you probably know, that wouldn't be a good idea.