sulfur corrosion of borosilicate glass
sulfur corrosion of borosilicate glass
(OP)
Does anyone know of any corrosion problems with elemental sulfur in contact with tempered borosilicate glass? Operating temperature is typically around 350F.
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
sulfur corrosion of borosilicate glass
|