INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Pinhole in HDPE pipe

Pinhole in HDPE pipe

Pinhole in HDPE pipe

(OP)
Hi,

I need some information regarding pinhole in HDPE gas pipe. I heard there is some information available in PPI.

Would anyone please let me know where I can find some pinhole information except ionixtechnologies info?

Thanks
Regards
Parvez

RE: Pinhole in HDPE pipe

I suspect you may be referring to the paper, "Static control in PE Fuel Gas Pipe", that I think has been published in many forms over several years (with maybe latest at http://www.ionixgastechnologies.com/Static%20Control%20in%20PE%20Fuel%20Gas%20Pipe.pdf).  In any case I suspect GTI (formerly GRI etc.), as a result of their research/data gathering etc., likely knows something about this subject (if you have access to this resource/information).

RE: Pinhole in HDPE pipe

(OP)
Thanks Conner.
Rgds
parvez

RE: Pinhole in HDPE pipe

(oops, I should have also mentioned "AGA")

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources