INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Shot Penning

Shot Penning

Shot Penning

(OP)
Good afternoon all:

I am in search of the Military shot penning spec.

MIL-13165

Does anyone know where i can get a copy of this?

Thanks guys

Bob
_innov8_

RE: Shot Penning

It is PEENING.

And here is the link:

assist.daps.dla.mil/quicksearch/

Regards,

Cory

Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.

RE: Shot Penning

Penning? The Military shot was already penned in many specs, but not in the MIL-13165.
cheers,

RE: Shot Penning

The spec is MIL-S-13165 and probably available
at your nearest technical library, university,
etc.

RE: Shot Penning

That would be "shot peening", not "penning".

Kenneth J Hueston, PEng
Principal
Sturni-Hueston Engineering Inc
Edmonton, Alberta Canada

RE: Shot Penning

What!!!  Did Corypad not cover the correct spelling adequately?

rmw

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources