INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

I need help

I need help

I need help

(OP)
hi, i have a little problem, We have to construct a earthfill with expansive clays, because it is the only material in the area for use.

What do you recommend to construct the little dam with this type of material? How can I isolate these?

Thank you very much for your help

RE: I need help

Don't spec a high percent compaction.   I'd go for placing it to the density it is found at,maybe like 82 percent Mod.Proctor.  Expect it will weaken, so make allowances in the slopes of embankments.

RE: I need help

Mix with lime at 4% by weight and see if the expansive quality is cured.  Place at 1-2% over optimum moisture using 90% compaction of a Standard proctor.  Alternate cure is cement adition, (try 5% by dry weight).  Cover backside/downstream face of embankment with sand/gravel filter drain and topsoil.

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources