Supplementary essential variable
Supplementary essential variable
(OP)
Dear All
I have a discussion open with a client:
Data:
Pressure vessel in compliance to Asme VIII ed 94 add 96
Material: Aisi 304
MDMT -196 °C
PQR with impact test at -196°C
Filler metal SFA 5.4
Question:
Are the supplementary essential variable required in the WPS?
My opinion is that I don't have to consider it, but due to the fact that for UHA-51(e)the impact test on weld metal is required my client require the application of the supplementary variable. Could you help me to understand if my client has reason?
Thanks in advance
PS I have posted this message in another section sorry for that
I have a discussion open with a client:
Data:
Pressure vessel in compliance to Asme VIII ed 94 add 96
Material: Aisi 304
MDMT -196 °C
PQR with impact test at -196°C
Filler metal SFA 5.4
Question:
Are the supplementary essential variable required in the WPS?
My opinion is that I don't have to consider it, but due to the fact that for UHA-51(e)the impact test on weld metal is required my client require the application of the supplementary variable. Could you help me to understand if my client has reason?
Thanks in advance
PS I have posted this message in another section sorry for that





RE: Supplementary essential variable
Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdoweb/
RE: Supplementary essential variable
Best regards - Al
RE: Supplementary essential variable