INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

questionable specification

questionable specification

questionable specification

(OP)
Is there anybody could come up with some idea about below valve material, or some related reference detail. Because i really have no idea about these valve material. Thanks a lot in advance!
1. BODY: 60K FORGED-DD-PSL2 TRIM: A182 F6A
2. BODY: 45K FORGED-BB-PSL2 TRIM: A182 F6A

 

RE: questionable specification

Body: Any forged material meeting the 60K PSL2 requirements of API 6A/ISO 10423

Trim: ASTM A182 F6A (UNS S41000) although a specific class will have to be specified for the actual heat treatment.

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdoweb/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources