CSA A23.1
CSA A23.1
(OP)
I just need to know the %age of air content for both moderate and severe exposure for max. agg. sie 3/4" for freezing and thwing exposure
When was the last time you drove down the highway without seeing a commercial truck hauling goods?
Download nowINTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: CSA A23.1
RE: CSA A23.1
For Category 1:
10mm agg: 6-9%
14-20mm agg: 5-8%
28-40mm agg: 4-7%
For Category 2:
10mm agg: 5-8%
14-20mm agg: 4-7%
28-40mm agg: 3-6%
RE: CSA A23.1
A please would have been nice!
RE: CSA A23.1
Thank you
RE: CSA A23.1
Dik