INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Yield and ultimate stresses for ASTM A668

Yield and ultimate stresses for ASTM A668

Yield and ultimate stresses for ASTM A668

(OP)
Hello:

I would greatly appreciate if someone can tell me the
yield stress (Fy) and ultimate stress (Fu) values of a steel ASTM A668 grad M.

Thank you and best regards.

RE: Yield and ultimate stresses for ASTM A668

It varies by thickness.  What size forgings are you looking at?

Tim

RE: Yield and ultimate stresses for ASTM A668

(OP)
Hello Constructioneer:

Thank you for your responding. The diameter is 6.5 in.

Regards.

RE: Yield and ultimate stresses for ASTM A668

Yield Point: 115 ksi
Min. Tensile: 140 ksi

Tim

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources