In the filling plant we use ozonated water, 3-5 ppm. Despite all talks with equipment manufacturers, we could not find resolute answer: which kind of gasket material is the bst ozone-resistant. Could anyone help with some advice.





RE: Ozone-Resistant Gasket
RE: Ozone-Resistant Gasket
Rated as Probally Satisfactory: Viton Extreme & EPDM P.C.
reference: metric-orings.com
see fluid compatability guide [reading}
RE: Ozone-Resistant Gasket
RE: Ozone-Resistant Gasket
RE: Ozone-Resistant Gasket
The first one is "Alcryn". This is a rubber product.
The second is "Flexible PVC".
Both of these materials are injection moldable.
The Alcryn is a great sealing material with great commpression set values.
Hope this helps.
Live Aloha