INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Low Temperature Ratings for Metals

Low Temperature Ratings for Metals

Low Temperature Ratings for Metals

(OP)
I'm looking for reference information regarding low temperature ratings for metals specifically 304,316,321, and 347 stainless steels.

RE: Low Temperature Ratings for Metals

In the case of API-650 tank construction, 304 and 316 may be used at any ambient temperature.  For pressure vessels, I think ASME VIII states that 304 and 316 may be used down to about -240F.  API-620 permits the use of SS for cryogenic temperatures, such as for LNG tanks.

Joe Tank

RE: Low Temperature Ratings for Metals

ASME BPV code gives temperature ratings for those materials.  I can't remember for sure, but I don't think you need any kind of impact testing down to at least -320, possibly lower.  

RE: Low Temperature Ratings for Metals

Please find the following limitation in ASME.

Temperature Limitation (deg.F) of Materials in ASME Code, up to add. 2004

Materials        Sec VIII-1        Sec VIII-2        B 31.3

304 SS            -320~1500    -320~800    -425~1500    
316 SS            -320~1500    -320~800    -425~ 800

321 SS            -320~1500    -320~800    -325~1500    
347 SS            -320~1500    -320~800    -425~1500

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources