16" SERIES "S" OWSJ info?
16" SERIES "S" OWSJ info?
(OP)
Anybody knows which manufacturer makes the 16" Series "S" owsj?
i need the capacity.
Building location is Toronto, Canada.
Thanks
i need the capacity.
Building location is Toronto, Canada.
Thanks






RE: 16" SERIES "S" OWSJ info?
RE: 16" SERIES "S" OWSJ info?
http://www.steeljoist.org/
RE: 16" SERIES "S" OWSJ info?
RE: 16" SERIES "S" OWSJ info?
can you share with me the specs for all 4 joists?
Thanks.
RE: 16" SERIES "S" OWSJ info?
Web members are designed to a minimum of 50% max shear
16S5 Resisting moment 202,000 in lbs.
Approximate weight 7.5 plf
Maximum end reaction 3,000#
16S6 Resisting moment 242,000 in lbs.
Approximate weight 8.5 plf
Maximum end reaction 3,300#
16S7 Resisting moment 290,000 in lbs.
Approximate weight 10 plf
Maximum end reaction 3,600#
16S8 Resisting moment 336,000 in lbs.
Approximate weight 11.5 plf
Maximum end reaction 3,900#
RE: 16" SERIES "S" OWSJ info?