INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

BMS 5-107

BMS 5-107

BMS 5-107

(OP)
We're going to repair B 737 floor panels. The SRM gives BMS 5- 107 (53-00-50) as the adhesive to use for the inserts. I can't find any reference anywhere for adhesives that meet this standard. It ought to be in 51-30-03 but it isn't.
Help!

Dan320

RE: BMS 5-107

Supplier specs. for BMS 5-107:

Araldite 420 A/B
or
Epibond 420 A/B
 

RE: BMS 5-107

Hi,

You can get a QPL (qualified suppliers list) for BMS 5-107 from myboeingfleet website. Normally, airlines / MRO who operates/maintains Boeing aircraft has access to this site.

The QPL contain the list of materials (in this case adhesive) meeting the specification with the corresponding supplier information.



Albert

RE: BMS 5-107

(OP)
Thank you guys. Really appreciate it.

Dan

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources