Magnetic properties of SS 416 (B-H)
Magnetic properties of SS 416 (B-H)
(OP)
Anyone knows where I can find the B-H curve of the SS 416 ?
Thanks!
Thanks!
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
Magnetic properties of SS 416 (B-H)
|
RE: Magnetic properties of SS 416 (B-H)
= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
RE: Magnetic properties of SS 416 (B-H)
Thanks
RE: Magnetic properties of SS 416 (B-H)
I make no claims to it's accuracy.
B (T) H (A/m)
0.000 0.0
0.200 318.3
0.426 477.5
0.761 795.8
1.097 1591.6
1.233 2387.3
1.335 3978.9
1.460 7957.8
1.590 15915.5
1.690 31831.0
1.724 44456.3
1.740 55704.3