INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

DAR structure book

DAR structure book

DAR structure book

(OP)
Hello all,

I am looking for a reference on stress applied to interior structures... I will give a more specific example...

I would like to analyse the airworthiness of an overhead bin on a A310 or B767. To do so, I need to provide a DAR with a structural report. I am looking for a guide book that will help me write this report. Something that will tell me which attachments to analyse, what type of stress to look for, what this stress will look like.

Thanks

RE: DAR structure book

Do a search for "Structural Substantiation".

RE: DAR structure book

i would have thought the DER would have been able to help you, other than that the guide book is probably FAR25 !

an overhead bin has lots of "issues" ... the baggage load, crasj loads (9g fwd, 3g side), flight loads (xg up/down ... this is probably the hardest one for find ... conservative guess is 9g), handling loads, materials (flammability).

once you've defined the strength requirements, it may be easier to test the thing rather than FE and composite panel analysis (but then i'm an old f**t who doesn't like composites much).

RE: DAR structure book

(OP)
thanks guys I found exactly what I was looking for in google: GAMA publication no.13: CABIN INTERIOR MONUMENT
STRUCTURAL SUBSTANTIATION METHODS

Thanks for the help

RE: DAR structure book

This company can approve your report

www.faader.us

Sigmatau

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources