Pressure Conductive Rubber
Pressure Conductive Rubber
(OP)
Can anybody help me in finding electrical conductive rubber which changes its el. resistance when pressed?
There is a known material called CS57-7RSC (CSA) from Yokohama, but it is hard to find some sample here in europe.
If somebody has knowledge/experience in this matter she/he would make me very happy by replying to this post.
There is a known material called CS57-7RSC (CSA) from Yokohama, but it is hard to find some sample here in europe.
If somebody has knowledge/experience in this matter she/he would make me very happy by replying to this post.





RE: Pressure Conductive Rubber
http:/
Since the patent was issued in 1981, it's expired (in the US), so maybe someone else can mix a similar composition for you.
Good luck!
Tom Jablonowski, TSE Industries, Inc.
www.tse-industries.com