West Texas Refinery
West Texas Refinery
(OP)
Does anyone have details of the cause of explosion on Feb 19, or any source of information?
Cheers,
gr2vessels
Cheers,
gr2vessels
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: West Texas Refinery
http://
http://www.inciweb.org/incident/1087/
http://www
RE: West Texas Refinery
It's utterly amazing that no one was killed when you look at the pictures of the refinery after the blast and see the damage.
RE: West Texas Refinery
I'd be curious what has actually failed, causing the leak. I'll be involved soon in a polypropylene plant upgrade and it would be instructive to learn from a such an event.
Be safe all,
cheers,
gr2vessels
RE: West Texas Refinery
RE: West Texas Refinery
cheers, gr2vessels
RE: West Texas Refinery
rmw
RE: West Texas Refinery