Quality SS MIM in China
Quality SS MIM in China
(OP)
Hi All,
I am looking for a small SS component in large qtys.
Can I take China into consideration, how is the quality of Chinese MIM SS components? Any concerns?
Please let me have any ideas for good producers with affordable prices.
Thanks!!!
I am looking for a small SS component in large qtys.
Can I take China into consideration, how is the quality of Chinese MIM SS components? Any concerns?
Please let me have any ideas for good producers with affordable prices.
Thanks!!!





RE: Quality SS MIM in China
You should also ask for the chinese equivalent of ISO 9000 Quality Management System.
http://www.welding-advisers.com/
RE: Quality SS MIM in China
Save water Drink Beer
RE: Quality SS MIM in China
RE: Quality SS MIM in China
I can't speak to the quality. Depends on what you want. If it's medical type work and is both small and intricate, my perception is that the quality is better in the States. Depends on what your liability is I guess.
RE: Quality SS MIM in China
I am indeed looking for a small part for a medical application. Please let me know if you have another producer you can think of.
RE: Quality SS MIM in China
Sorry to be so rough on the asians, but I have been burned before and you can't ignore the issues that keep coming from there about quality.
RE: Quality SS MIM in China
RE: Quality SS MIM in China
Dave Hyman
Mechanical Engineer
RE: Quality SS MIM in China