Responsability for Pressure Piping per ASME B31.3 fabrication
Responsability for Pressure Piping per ASME B31.3 fabrication
(OP)
Hi,
I have to weld (fabrication) a pressure piping per ASME B31.3. I work in Quebec, Canada and the product will be installed in Saskatchewan, Canada. After welding the client ask to do the spot radiography inspection and hydro test on its own.
What is my the responsability regarding the code and the client if he has done the conception?
From what I know; traceability and a qualified Inspector followed fabrication and inspection is my responsability. (what else, if I miss something...)
Thanks
I have to weld (fabrication) a pressure piping per ASME B31.3. I work in Quebec, Canada and the product will be installed in Saskatchewan, Canada. After welding the client ask to do the spot radiography inspection and hydro test on its own.
What is my the responsability regarding the code and the client if he has done the conception?
From what I know; traceability and a qualified Inspector followed fabrication and inspection is my responsability. (what else, if I miss something...)
Thanks





RE: Responsability for Pressure Piping per ASME B31.3 fabrication
What do your contract documents state regarding this job?
RE: Responsability for Pressure Piping per ASME B31.3 fabrication
RE: Responsability for Pressure Piping per ASME B31.3 fabrication
http://www.ihs.com/
RE: Responsability for Pressure Piping per ASME B31.3 fabrication
http://w
Looks like SK has a Boiler and Pressure Vessel Act that will cover this as well.
http://w
Based on random search of provincial site, so verify before using
SLH