INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

How long to keep PWHT Records?

How long to keep PWHT Records?

How long to keep PWHT Records?

(OP)
I need to set a time limit on keeping PWHT records.
These are for modifications and repair work of low carbon steel piping in an alumina refinery.
I am looking for some idea of what other people do so I can be realisitic (rather than keep everything)
I am thinking 5 years -  does that sound reasonable?

Thanks in advance.
  John

RE: How long to keep PWHT Records?

5 years is in line with ISO 29001 used by the oil & gas industry

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdoweb/

RE: How long to keep PWHT Records?

(OP)
Thanks for that Steve. Nice and concise!  
Good to know there is a standard to refer to.
Cheers,  John

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources