INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

API-5L-B, DSAW / A672 GR.60 CLASS 22

API-5L-B, DSAW / A672 GR.60 CLASS 22

API-5L-B, DSAW / A672 GR.60 CLASS 22

(OP)
Hi,

I am reading a specification giving me the choice between two type of pipe, API-5L-B, DSAW or A672 Gr.60 Class 22.  Does somebody knows what is the major mechanical difference between this two kind of pipe ?

Thanks

RE: API-5L-B, DSAW / A672 GR.60 CLASS 22

SMYS - API GrB: 241  A672 Gr60: 220 (Assuming that you are comparing PSL 1)

A670 Cl22 is in the stress relieved condition whereas 5L B is unlikely to be.  

Steve Jones
Materials & Corrosion Engineer
http://www.pdo.co.om/pdoweb/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources