INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

304 Stainless Stress Values

304 Stainless Stress Values

304 Stainless Stress Values

(OP)
Hello All,
I know that this is probably a pretty basic question, however, I have just started to work with the Pressure Vessel Code. Where are the stress tables for 304L located?

RE: 304 Stainless Stress Values

(OP)
I was able to locate them via the online tables.

RE: 304 Stainless Stress Values

Well everything you need is in BPVC SecII D, and it is an amazing collection of information.

Paul
www.ostand.com

RE: 304 Stainless Stress Values

Section II, Part D, Table 1A.

RE: 304 Stainless Stress Values

gmarken (Mechanical):

For material occurs in ASME II-D (table 1A) tables more than once be careful of note G5 (as in table 1a Notes) especially when dealing with austenitic SS like 304.

-jehan

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources