INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

A106 GrB- A106 GrB

A106 GrB- A106 GrB

A106 GrB- A106 GrB

(OP)
Hi all

My question is considerably simple

What is the difference between A106Gr A and A106Gr B

Thanks

RE: A106 GrB- A106 GrB

basically

tensile
yield
allowable stress

small chemistry difference

i can't remember the last time I saw gr A specified

RE: A106 GrB- A106 GrB

(OP)
Do you know the exact values of tensile, yield and allowable stress for A106GrB and A106GrA

RE: A106 GrB- A106 GrB

ntaylak

From Table A-1 of B31.3, Appendix A

ASTM A-106, Grade A
Tensile strength - 48 KSI
Yield strength - 30 KSI

ASTM A-106, Grade B
Tensile strength - 60 KSI
Yield strength - 35 KSI

Regards, John

RE: A106 GrB- A106 GrB

(OP)
Thanks A lot Jonh

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources