INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Nylon Spacers
4

Nylon Spacers

Nylon Spacers

(OP)
Hello everybody,
I am looking for a nylon spacer for a 2-56 machine screw with a length of 9/32" or 7mm. I have been looking all over but all I can find is a version on McMaster which is over a dollar per spacer, I could get them machined locally for probably less. So if anybody has an idea, maybe in China, please let me know.
Thank you very much in advance
Domenic

RE: Nylon Spacers

(OP)
thank you, but I have tried them already they didn't have the length I need

RE: Nylon Spacers

How about Micro Plastics - They are really fast at sending out samples.

https://secure.microplastics.com/catalogpictorial.aspx

Heckler   americanflag
Sr. Mechanical Engineer
SWx 2007 SP 4.0 & Pro/E 2001
      o
  _`\(,_
(_)/ (_)

This post contains no political overtones or undertones for that matter and in no way represents the poster's political agenda.

RE: Nylon Spacers

By samples from Mcmaster, and see if there is a manufacturer named on the package.

RE: Nylon Spacers

The Tick has a good point.  I've bought stuff from McMaster Carr and it comes in the original mfg packaging.....then I know the supplier.  I've only been able to get the supplier from a MMC rep once and it was only because they didn't carry the size I needed.

Heckler   americanflag
Sr. Mechanical Engineer
SWx 2007 SP 4.0 & Pro/E 2001
      o
  _`\(,_
(_)/ (_)

This post contains no political overtones or undertones for that matter and in no way represents the poster's political agenda.

RE: Nylon Spacers

(OP)
thx a lot guys, but once again I have also looked through microplastics and 9/32 seems to be a real oddball. I will however try the sample method.
Cheers

RE: Nylon Spacers

Not necessarily right for your situation but…

At my place we’ll often pick parts out of McMaster, order enough for prototypes etc.

When it gets into production our purchasing people frequently get an equivalent item from a local hardware supplier (http://www.specialtytoolandbolt.com/).  [Don’t get me started on how equivalent is determined…]

So do your purchasing people have a preferred supplier you could go to, or have you already asked them/doesn’t apply to your situation?

KENAT, probably the least qualified checker you'll ever meet...

RE: Nylon Spacers

(OP)
a qoute to local suppliers is out at the moment so we are waiting to hear back from them.
thanks for the quick reply

RE: Nylon Spacers

I would give Bokers a call assuming any quanity.
They have sent me a sample packet that included the one off size I needed.

http://www.bokers.com/

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources