HIGH TENSILE STEEL
HIGH TENSILE STEEL
(OP)
HI
I GENRALLY HEARED PEOPLE IN INDIAN INDUSTRIES USE A TERM HIGH TENSILE STEEL
BUT CAN ANYONE CLARIFY ME ABOVE WHAT TENSILE STRENGTH(PSI) WE CAN SAY IT IS HIGH TENSILE
I GENRALLY HEARED PEOPLE IN INDIAN INDUSTRIES USE A TERM HIGH TENSILE STEEL
BUT CAN ANYONE CLARIFY ME ABOVE WHAT TENSILE STRENGTH(PSI) WE CAN SAY IT IS HIGH TENSILE





RE: HIGH TENSILE STEEL
It varies depending on the industry. I would say that for the boiler and pressure vessel industry, an ultimate tensile strength of 90 Ksi and higher would be considered high strength.
RE: HIGH TENSILE STEEL
Regards,
Cory
Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.