INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Ethylene Guard Bed for Polyethylene Batch Reactor

Ethylene Guard Bed for Polyethylene Batch Reactor

Ethylene Guard Bed for Polyethylene Batch Reactor

(OP)
Gentlemen,

We have a small scale polyethylene batch reactor used to test the performance of a comonomer (1-Octene). We use ethylene straight off our ethylene recovery plant, but are not really in the polyethylene business (at this site at least).

At a meeting this morning I was told that the customer was wondering why we did not guard bed our ethylene before the reactor to insure that our comonomer was run under the best possible conditions. It was proposed that ethylene feed guard beds were standard even in polyethylene plants that recieve polymer grade pipeline ethylene such as ours.

Is there anyone with polyethylene experience that can tell me if this information (feed ethylene guard bedding) is true? I would also appreciate some details as to what guard bed material is used, and what poisons are being targeted (acetylene, CO, methanol, etc).

best wishes always,
ssehp

RE: Ethylene Guard Bed for Polyethylene Batch Reactor

I'll get you started, I'm not a polymer engineer, but I delivered billion of pounds of ethylene and here are the problems we were asked to look into.

Sulphurs of course, poison catalysts.
CO2 is a polymer stopper, CO2 should be under 2 ppm.
Ammonia, it is found in refinery ethylene.
Water
Acetylenes.
Ethane and methane are inerts and just build up over time.

The gaurd beds are typically a ZnO to remove Sulphur, Mole sieves to remove water and CO2.  

I don't remember what was the agent for ammonia.

The Catalyst handbook by Twigg has some good info.

RE: Ethylene Guard Bed for Polyethylene Batch Reactor

(OP)
DCasto,
Thanks for the advice. I have just ordered a copy of Twigg's "The Catalyst handbook". I may owe you a star.
best wishes,
sshep

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources