Thermal Properties
Thermal Properties
(OP)
I am new to this forum and Boilers. I am looking for thermal properties (thermal conductivity, specific heat and etc) of various parts of a boiler. Any lead on this greatly appreciated.
Thanks.
Thanks.





RE: Thermal Properties
Thermal conductivity data can be found in the ASME Boiler & Pressure Vessel Code, Section II, Part D, Subpart 2.
RE: Thermal Properties
Here is basic enthalpy vs temperature plot for ten (10) species:
Here is a URL for free calculators dealing with physical properties for a few species:
http://members.aol.com/engware/calc1.htm
I do hope that you will find the above plot and a URL for online calculators useful.
Thanks,
G. Feric, PE
http://engware.i-dentity.com