INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Fastener Head Marking
2

Fastener Head Marking

Fastener Head Marking

(OP)
Does anybody recognise the manufactures marking "LM" on the head of a fastener - image attached

RE: Fastener Head Marking

(OP)
I looked through the MIL document before I posted and the marking was not clearly identified. There is an "LM" shown for Levingstom Machine Company, Haltom City, Texas but the shape of the lettering is different.

RE: Fastener Head Marking

The marking of 3 radial lines indicates a Grade 5 bolt (SAE J429 Grade 5). Based on information I have, the "LM" mark likely belongs to a factory in China by the name of Ningbo Haixin Hardware.

RE: Fastener Head Marking

(OP)
Billybaru - Do Ningbo Haixin use a number of head-stamps? I thought their marking was "HX".

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources