INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Delrin 111P NC010 fatigue curve

Delrin 111P NC010 fatigue curve

Delrin 111P NC010 fatigue curve

(OP)
Hello to all forum, there is someone that can give me or said where find the fatigue curve about Delrin 111P NC010 or other kind of Delrin?
On Dupont web site there aren't these information

Regards
Stefano

RE: Delrin 111P NC010 fatigue curve

Here a link to an excellent design guide for Delrin

http://www.distrupol.com/downloads/Delrin(TM)_POM_Moulding_manual.pdf

No mention of fatigue though. You'll have to ask an actual person at DuPont. They probably do have the data.

There is not any memory with less satisfaction than the memory of some temptation we resisted.
- James Branch Cabell

RE: Delrin 111P NC010 fatigue curve

DuPont will certainly have the data. As Demon3 says, you will need to contact a real person there, preferably a technical support person.

You get more data if you can find an old technician as often data at that level is no longer in print as the marketing guru's tend to think it looks complicated and scares off prospective customers. They don't seem to consider the counterpoint that those scared of by real data are often headed for a disaster, and without the data to scare them off will charge on regardless. These disasters cost everyone involved.

Regards

eng-tips, by professional engineers for professional engineers
Please see FAQ731-376: Eng-Tips.com Forum Policies for tips on how to make the best use of Eng-Tips Fora.

RE: Delrin 111P NC010 fatigue curve

This book should have it. I have the version for PP and it contains fatigue data.

http://www.amazon.com/Tribological-Properties-Plastics-Elastomers-Handbook/dp/1884207154

Fatigue and Tribological Properties of Plastics and Elastomers (PDL Handbook Series) (Hardcover)

For all practical purposes, the useful life of a plastic component is equal to its fatigue life under conditions of cyclic loading such as those that occur in vibration. Equally important to materials engineers and designers are abrasion, friction and wear - tribological properties. Over 80 generic families are covered including thermoplastics, thermosets, thermoplastic elastomers and rubbers. Neat resins, blends and alloys, plastics with various combinations of fillers, additives and more are covered. Also covers plastics mated to plastics and metals.

There is not any memory with less satisfaction than the memory of some temptation we resisted.
- James Branch Cabell

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources