JIS Material Standards
JIS Material Standards
(OP)
Help! I have a drawing for a number of pump parts that I need to manufacture for my customer. His company purchased the pump from a Japanese supplier. All the drawings are in metric (which is not a problem) but the notes are in Japanese (which is a problem). Can anyone tell me what the following materials are?
SS41
S35C
S25C
WJ2
Thanks,
sqearly
SS41
S35C
S25C
WJ2
Thanks,
sqearly





RE: JIS Material Standards
- S25C (SAE 1025) and S35C (SAE 1035) : You should refer to JIS G4051.