INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS

Log In

Come Join Us!

Are you an
Engineering professional?
Join Eng-Tips Forums!
  • Talk With Other Members
  • Be Notified Of Responses
    To Your Posts
  • Keyword Search
  • One-Click Access To Your
    Favorite Forums
  • Automated Signatures
    On Your Posts
  • Best Of All, It's Free!
  • Students Click Here

*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail.

Posting Guidelines

Promoting, selling, recruiting, coursework and thesis posting is forbidden.

Students Click Here

Jobs

Vacuum Pump Vanes

Vacuum Pump Vanes

Vacuum Pump Vanes

(OP)
I am looking for new vane material for a sliding vane vacuum pump for chemical applications. I know composites are used for this application, but don't know materials or suppliers. Can someone give an assist?

RE: Vacuum Pump Vanes

American Matrix Corp make such materials.  We pake stock plates using continious carbon fiber and PEEK or PPS thermoplastic resin.  Visit our web site at www.americanmatrixcorp.com for more information about the material.  You can contact me at rmdavies@americanmatrixcorp.com

RE: Vacuum Pump Vanes

i am supplying material for vanes application which suits most needs.

contact me at t_innovative@hotmail.com

my address

J K ARORA
EINNOVATIVE TECHNOLOGIES
9,AVIS ENCLAVE
DSOUZA COLONY
NASIK-422005
INDIA

RE: Vacuum Pump Vanes

Our company manufactures carbon-graphite vanes, with phenolic impregnation.  The cost will be much lower than composite materials, and chemical resistance is very good.

RE: Vacuum Pump Vanes

(OP)
Please send me the name of your company.

RE: Vacuum Pump Vanes

If you are still interested in these types of materials.  My company has vane products that have the best chemical resistance of any material, service tempertures to 550F, low friction, near 0 thermal expansion, flex strength of 135ksi and flex modulus of 7.5msi.  Email your requirements to rmdavies@americanmatrixcorp.com. Web site at www.americanmatrixcorp.com for more information about the material.

RE: Vacuum Pump Vanes

I need vanes for hydraulic motor application. The medium is hydraulic oil. Pressures range upto 100 kg/cm2. I will appreciate if I know the material to be used for such vanes. Thanks

RE: Vacuum Pump Vanes

We specialise in pump vanes from many composite materials, for your application a vane from our Max Performance Vanes
would seem appropriate. Please contact me or visit our site at aavf.co.uk
Darrian

Red Flag This Post

Please let us know here why this post is inappropriate. Reasons such as off-topic, duplicates, flames, illegal, vulgar, or students posting their homework.

Red Flag Submitted

Thank you for helping keep Eng-Tips Forums free from inappropriate posts.
The Eng-Tips staff will check this out and take appropriate action.

Reply To This Thread

Posting in the Eng-Tips forums is a member-only feature.

Click Here to join Eng-Tips and talk with other members!


Resources