hard chroming
hard chroming
(OP)
Does anybody have any sources preferably Canadian, or Northern US that can wear chrome a feeder housing 45" x 45" x 45"
INTELLIGENT WORK FORUMS
FOR ENGINEERING PROFESSIONALS Come Join Us!Are you an
Engineering professional? Join Eng-Tips Forums!
*Eng-Tips's functionality depends on members receiving e-mail. By joining you are opting in to receive e-mail. Posting GuidelinesJobs |
|
RE: hard chroming
In Cleveland, Ohio there is Master Chrome Service at http://www.masterchromeservice.com/. We have used them for driveline shafts, but the web site reports capability of handling items up to three tons.