Creep Temperature (Creep cracking)
Creep Temperature (Creep cracking)
(OP)
Hi,
I'm Xeros.
each material has specific creep temperature.
So, my client request the creep temperature for Cr-Mo steel and 25Cr-35Ni steel.
I could find web site for provide the creep temperature for material.
However, i think that data on web-site is not enough for reference to client.
Please give me the information about reference book title, code, standard or specification.
Best regards,
I'm Xeros.
each material has specific creep temperature.
So, my client request the creep temperature for Cr-Mo steel and 25Cr-35Ni steel.
I could find web site for provide the creep temperature for material.
However, i think that data on web-site is not enough for reference to client.
Please give me the information about reference book title, code, standard or specification.
Best regards,





RE: Creep Temperature (Creep cracking)
"Report on the Elevated-Temperature Properties of Chromium-Molybdenum Steels" Special Technical Publication No.151
For 25Cr-35Ni steels go here;
http://tsuge.nims.go.jp/top/creep.html
Note;
RE: Creep Temperature (Creep cracking)
- API RP579, Table 4.1
- API STD 530, Annex E