Allowable Compressive Stress at High Temperatures
Allowable Compressive Stress at High Temperatures
(OP)
Can anyone suggest a method or provide data for determining allowable compressive stress for a cylinder of specific geometry operating at a temperature above the limits in ASME Section II, Part D, Subpart 3?
The specific application would be a tall column constructed of SA-516-70 material receiving local band PWHT and subject to axial and wind loads. PWHT temperature for design purposes would be 1200F. Thanks.
The specific application would be a tall column constructed of SA-516-70 material receiving local band PWHT and subject to axial and wind loads. PWHT temperature for design purposes would be 1200F. Thanks.





RE: Allowable Compressive Stress at High Temperatures
RE: Allowable Compressive Stress at High Temperatures
Joe Tank